Local, distortional and global buckling of cold-formed steel, explained
The three ways a thin-walled steel member buckles, how to tell them apart on a signature curve, and how AISI S100-24 turns each into a strength. With finite strip results for a real stud.
- Thin-walled steel members buckle in three ways: local (the flat walls ripple in short waves), distortional (a flange and its lip rotate about the web–flange corner) and global (the whole member bends or twists between braces).
- Each mode has its own buckle length. A finite strip signature curve plots the buckling load against that length, and its minima give the local and distortional buckling loads.
- AISI S100-24 checks all three: global buckling in §E2 and §F2, local buckling interacting with global buckling in §E3 and §F3, and distortional buckling in §E4 and §F4. The lowest strength governs.
- For a 362S162-54 stud in compression, the finite strip analysis gives local buckling at 15.82 kip and distortional buckling at 23.46 kip, against a squash load of 21.10 kip.
Hot-rolled steel shapes are thick enough that, for most members, the question is when the steel yields or the member buckles as a whole. Cold-formed studs, joists and purlins are bent from sheet 0.03 to 0.12 in thick. Their walls are so slender that they can buckle locally at a fraction of the yield stress, long before the member as a whole is in trouble. That is the single biggest difference between cold-formed and hot-rolled design, and it is why AISI S100 spends most of its member chapters on buckling.
This article explains the three buckling modes, shows them for a real section, and connects each one to the clauses of AISI S100-24 that turn it into a strength.
The three modes at a glance#
| Mode | What moves | Typical half-wavelength | Post-buckling reserve | S100-24 sections |
|---|---|---|---|---|
| Local | The flat plates between corners ripple; the corners stay straight | About the width of the widest plate | Large | §E3, §F3 |
| Distortional | A flange and its lip rotate about the web–flange corner; the cross-section changes shape | Several times the plate widths | Moderate | §E4, §F4 |
| Global | The whole cross-section moves as a rigid shape: bending, twisting or both | The unbraced length of the member | Small | §E2, §F2 |
The half-wavelength is the length of one buckle along the member. It matters because each mode has its own preferred length, and that is what lets an analysis tell them apart.
Local buckling#
Picture the web of a stud as a long, thin plate supported along its two edges by the flanges. Under compression it buckles into a series of short waves, each roughly as long as the web is deep. The corners don't move: they act as the plate's supports.
Local buckling does not mean failure. A buckled plate keeps carrying load through its stiffer edges, which is the idea behind the effective width of a plate: the buckled middle of the plate sheds stress to the edges. This post-buckling reserve is why a cold-formed section can carry well above its local buckling load.
Distortional buckling#
A lipped flange is held at one edge by the web and at the other by a short lip. Neither support is rigid. If the web is slender and the lip is short, the flange and lip can rotate together about the web–flange corner, and the cross-section changes shape. That is distortional buckling.
Its buckles are longer than local buckles (several times the flange width) and its post-buckling reserve is smaller. Distortional buckling is the reason the lip length of a stud is not arbitrary, and the reason that bridging, sheathing and blocking matter even when a member is laterally braced. A brace or sheathing that holds the flange can restrain it.
Global buckling#
Global buckling is what most engineers learn first: flexural, torsional and flexural-torsional buckling of columns, and lateral-torsional buckling of beams. The cross-section keeps its shape and moves as a whole over the unbraced length. Because a C or Z section's shear center is offset from its centroid, twisting and bending couple, and flexural-torsional buckling often governs the weak-axis behaviour of a C-stud.
Seeing the modes: the signature curve#
The clearest way to see all three is a finite strip analysis. It finds the buckling load of the cross-section for a range of buckle half-wavelengths, with the ends of each buckle simply supported. Plotting the load against the half-wavelength gives the signature curve. Hancock introduced the idea for I-beams, and Schafer's free CUFSM program made it routine for cold-formed sections.
Here is the signature curve of a 362S162-54 stud (3-5/8 in deep, 54 mil) in pure compression, computed by ColdCalc:
Read it from left to right:
- At short half-wavelengths the curve falls to a minimum at about 2.8 in. That is local buckling, and the load there is Pcrℓ = 15.82 kip.
- The curve rises, then falls to a second minimum at about 13.7 in. That is distortional buckling: Pcrd = 23.46 kip.
- Beyond that the curve keeps falling as the member gets longer. That is global buckling, and for a real member you read it at the unbraced length.
The squash load of this stud is Py = A·Fy = 21.10 kip, so its local buckling load is below its yield load: the walls buckle before the steel yields, and the post-buckling reserve carries the rest.
The same analysis gives the buckled shape at each minimum. Local buckling ripples the web and flanges, while the corners stay put. Distortional buckling swings the flange and lip about the corner:
When the curve has no clear minimum#
Not every section is so tidy. Make the web deeper and the distortional minimum can merge into the rising local branch or the falling global branch. Here is the 6 in deep 600S162-54 in compression:
There is a shoulder where distortional buckling should be, but no dip. Labelling minima by eye fails here, and a program that only looks for two minima would miss the distortional mode or take the wrong point. The constrained finite strip method (cFSM) solves this by measuring how much of each buckled shape is local, distortional or global. It finds the distortional mode at 16.4 in with Pcrd = 12.72 kip. Its local buckling load, 7.81 kip, is only about a quarter of its squash load of 27.82 kip.
ColdCalc labels every minimum by its modal participation for this reason. The finite strip article covers how it works.
From buckling loads to strength in AISI S100-24#
Elastic buckling loads are not strengths. The Specification turns them into nominal strengths with equations calibrated on tests, and it treats the three modes differently:
- Global: §E2 for columns gives Pne from the global buckling stress Fcre. §F2 for beams gives Mne. Appendix 2 §2.3 has the closed-form expressions for Fcre, or you can take it from a finite strip analysis at the member's length.
- Local: local buckling interacts with global buckling. A column that is already buckling globally has lower stresses at which its plates buckle, so §E3.2 caps the local strength at Pne, not Py. With the Effective Width Method (§E3.1 with Appendix 1), the same idea appears as the effective area at the global stress Fn.
- Distortional: §E4 and §F4 check distortional buckling against the yield load. They assume it does not interact with global buckling.
The member's strength is the smallest of the three. For either stud above as a short column, the local (§E3.2) and distortional (§E4) strengths come out within a few percent of each other, so either can govern: a reminder that neither check can be skipped. The Direct Strength Method article works through the numbers with the new S100-24 equations.
What this means in practice#
- Lighter is not always weaker in proportion. A thinner stud loses strength faster than its area because its walls buckle earlier.
- Bracing does more than shorten the global length. Bridging and sheathing that hold the flanges also raise the distortional strength. S100-24 accounts for this through a rotational stiffness kφ in Appendix 2 §2.3.3.
- Lip length matters. Too short a lip lets the flange distort. SSMA lip lengths and the B4 limits of S100-24 keep sections in the range where the equations were calibrated.
- Holes change local and distortional buckling. Web punchouts lower both Pcrℓ and Pcrd. S100-24 has provisions for both methods.
What is distortional buckling in cold-formed steel?
Distortional buckling is a mode in which a flange and its edge stiffener (lip) rotate about the web-flange corner, so the cross-section changes shape. Its buckles are longer than local buckles and shorter than global ones, and it has less post-buckling strength than local buckling. AISI S100-24 checks it in Sections E4 (compression) and F4 (bending).
What is the difference between local and distortional buckling?
In local buckling the flat plates ripple in short waves while the corners stay in place. In distortional buckling the corners move: the flange and lip rotate about the web-flange junction. Local buckles are about as long as the plate is wide; distortional buckles are several times longer.
How do I find the local and distortional buckling loads of a section?
Run a finite strip analysis (for example CUFSM or ColdCalc) to get the signature curve, and read the local and distortional minima. For simple shapes, AISI S100-24 Appendix 2 also gives closed-form expressions. Constrained finite strip (cFSM) modal identification helps when the minima are not distinct.
Does local buckling mean a cold-formed member has failed?
No. Thin plates have substantial post-buckling strength, so a member usually carries well above its elastic local buckling load. The Direct Strength and Effective Width Methods in AISI S100-24 account for that reserve.